Filler Metal ALLOY 625 is used for gas-metal-arc-welding (Mig) of alloy 625, alloy 825, alloy 25-6MO, and a range of high alloy austenitic and super austenitic stainless steels. It is also used for surfacing of steel, for welding 9% Ni steels, and for welding various corrosion-resistant alloys such as alloy 20.
Filler Metal 625 can be used for joining and overlaying with Submerged Arc process. The weld metal has high strength over a broad temperature range and has resistance to localized attack such as pitting and crevice corrosion.
Filler Metal 625 is useful for many dissimilar joints involving INCONEL® and INCOLOY® alloys, carbon steels, low-alloy steels, and stainless steels.
Typical Mechanical Properties:
Tensile Strength: MPa 760 (psi 110,000)
Elongation, (4d) % 30
Filler metals available on spool in a variety of sizes and diameters
Element | Value |
---|---|
Cr | 20-23 |
Ni | 58 min |
C | 0,10 max |
Mn | 0,5 max |
Si | 0,5 max |
Fe | 5,0 max |
Cu | 0,50 max |
Ti | 0,40 max |
Nb | 3,15-4,15 |
Mo | 8-10 |
Co | 1,0 max |