MENU
ALLOY 60 Mig Welding Wire Filler Metal

ALLOY 60 Mig Welding Wire Filler Metal

Filler Metal Alloy 60 is used for gas-metal-arc-welding (Mig), and submerged-arc welding of MONEL® alloys 400, R404, and K-500.
It is also used for surfacing of steel by the gas-metal-arc or submerged-arc processes.
For certain gas-metal-arc conditions, a barrier layer of Nickel Filler Metal Alloy 61 is recommended.
Weld metal deposited by Filler Metal Alloy 60 has properties similar to those of MONEL® alloy 400. It has good strength and resists corrosion in many media, including sea water, salts, and reducing acids.
The weld metal is not age hardenable and when used to join MONEL® alloy K-500 has lower strength than the base metal.

Typical Mechanical Properties:
Tensile Strength: MPa 480 (psi 70,000)
Elongation, (4d) % 30

Filler metals available on spool and in a variety of sizes and diameters.
AWS A5.14 ERNiCu-7 - (UNS N04060)
Chemical analysis
Element Value
Ni 62-69
C 0,15 max
Mn 4,0 max
Si 1,25 max
Fe 2,5 max
Cu Bal.
Ti 1,5-3,0
Al 1,25 max


Packaging
Item Packaging
ALLOY 60 (ER NiCu-7) As required